PETG is the default pick for most RC and drone parts. ASA is the pick when the part lives outdoors in sun and weather. Nylon is the toughest of the three, and the hardest to print, so it belongs on high-load brackets, gears, and wear parts once you can keep it dry and enclosed. First functional part on an open-frame printer? Start with PETG. Part sits in sun all summer? Print it in ASA. Repeated load and failure is not an option? Nylon earns its extra work.
How to read the numbers in this guide
Datasheet figures vary by brand, grade, test method, and moisture state, so this guide does not mix brands into one table. The comparison table below is qualitative on purpose. Where a figure is given, it comes from one named manufacturer datasheet and describes a lab specimen printed at 100 percent infill, not your part. For PLA and PLA+ basics, read the PLA guide first: PLA vs PLA+ vs PETG: Pick the Right 3D Printer Filament for Drone Parts.
Is PETG good for RC and drone parts?
Yes. PETG is the easy engineering filament and the baseline for rigid drone and RC parts. It prints on most printers without an enclosure, flexes instead of snapping, and holds up better than PLA under knocks, heat, and water. The listing for the stocked PETG refill states impact resistance twice that of standard PLA, with enhanced chemical and water resistance. That figure comes from the live listing.
Heat: PETG handles more heat than PLA but less than ASA or nylon. Polymaker lists 69C and Bambu Lab lists 71C for its PETG Basic, both heat deflection at 0.45 MPa.
Strength: PETG is strong and a little flexible. It bends under load instead of cracking through, and its layers hold together better than any other common filament. CadFlow, using Polymaker datasheets, lists PETG at 48 MPa printed flat and 45.7 MPa printed upright, so it keeps about 95 percent of its strength across the layers.
Warping and enclosure: PETG warps little and needs no enclosure. Fumes: none special.
Settings: typical ranges across the Filwiz, Techietory, and ADP guides are nozzle 230 to 250C, bed 70 to 80C, fan 30 to 60 percent. Too much cooling weakens layer adhesion.
Weaknesses: PETG strings more than PLA, so tune retraction until the strings stop. It bonds hard to a bare bed, so use a release agent such as a glue stick on smooth PEI. Damp PETG prints rough and weak, so dry it at about 65C for 4 to 6 hours if you hear popping.
Is ASA good for RC and drone parts?
Yes, when the part lives outdoors. ASA is essentially ABS with UV resistance built in. It was developed to fix the weakness that kills ABS outside: yellowing and brittleness after sun exposure. If your part goes outdoors, ASA is the default choice, and every top guide agrees on that point.
Heat: ASA handles more heat than PETG by a clear margin. Polymaker lists 103C and Bambu Lab lists 100C for its ASA, both heat deflection at 0.45 MPa.
Strength: ASA is tough on impact and rigid enough for structural parts, but it is not stronger than PETG in a straight pull. Polymaker lists ASA at 43.8 MPa printed flat and 32 MPa printed upright, against PETG at 48 and 45.7 MPa. Pick ASA for sun and heat, not for raw tensile strength.
UV and weather: this is the reason ASA exists. It holds its color and structure under UV, where ABS yellows and turns brittle and PLA breaks down in direct sunlight over time. Use ASA for antenna mounts, drone housings, and RC car bodies.
Warping and enclosure: ASA warps significantly without an enclosure, and it is the number one ASA printing problem across the guides. It shrinks as it cools, so drafts cause warping and layer splitting. An enclosure is strongly recommended, with a warm chamber around 35 to 50C. A brim of 5 to 10 mm helps on large parts.
Fumes: ASA emits styrene fumes while printing, so ventilation is required, not optional. Print in a well-ventilated area or exhaust the fumes outside. A carbon filter is the minimum for ASA, per the Filwiz guide.
Settings: typical ranges across the Filwiz, Techietory, and ADP guides are nozzle 240 to 260C, bed 90 to 110C, fan 0 to 30 percent, print speed 40 to 80 mm per second.
Weaknesses: without an enclosure ASA warps and splits, and with too much fan it cracks between layers. It costs about a third more per spool than PETG, per the CadFlow price check.
Is nylon good for RC and drone parts?
Yes, for the hardest jobs, and only if you respect its moisture problem. Nylon, also called polyamide or PA, offers the best combination of tensile strength, impact resistance, and abrasion resistance of any common FDM filament. It bends instead of shattering, resists wear, and is slippery enough for gears, bushings, and living hinges. It is also the hardest of these three materials to print.
Heat: nylon handles more heat than PETG and about the same as ASA, with the exact figure depending on grade and annealing. Polymaker lists its nylon copolymer at 111C heat deflection after annealing, the highest of the six filaments CadFlow compared.
Strength: nylon is the strongest of the three in a straight pull and the toughest on impact. CadFlow lists 78 MPa printed flat and 45.8 MPa printed upright, only 59 percent of its flat strength across the layers. Orientation matters most for nylon: print a nylon hook lying down, not standing up.
Wear: nylon is the pick for parts that slide, rub, or hinge. Gears, hinges, bushings, snap-fit clips, wear plates, and living hinges are nylon jobs. A nylon part does not shatter. It bends, absorbs the hit, and returns to shape
Warping and enclosure: nylon warps severely without an enclosure. An enclosure is required, with a warm chamber around 45 to 65C, and a large brim plus a Garolite bed surface helps adhesion.
Moisture: this is the nylon problem that decides everything else. Nylon absorbs moisture from the air fast, and wet nylon prints with popping, stringing, rough surfaces, and weak layer bonds. Filwiz cites up to 9.5 percent moisture by weight for PA6 and Prusa lists up to 10 percent, while CadFlow cites 2.82 percent for Polymaker PolyMide CoPA. Dry it at 70 to 80C for 6 to 12 hours before printing, and print from a dry box if possible.
Settings: typical ranges across the Filwiz, Techietory, and ADP guides are nozzle 240 to 290C depending on grade, bed 70 to 90C, fan 0 to 30 percent, print speed 30 to 60 mm per second. Filled nylon needs a hardened steel nozzle.
Weaknesses: wet filament, no enclosure, and wrong orientation are the three killers. Upright orientation throws away nearly half its strength.
How do PETG, ASA, and nylon compare side by side?
| Property | PETG | ASA | Nylon (PA6 / PA12) |
|---|---|---|---|
| Easiest to print | Easiest of the three | Moderate, needs enclosure | Hardest of the three |
| Heat resistance | Moderate, better than PLA | High, best for sun and hot cars | High, best after annealing |
| Strength in a straight pull | Strong | Strong, slightly below PETG | Strongest of the three |
| Strength across the layers | Best, about 95 percent of flat strength | Weaker, about 73 percent of flat strength | Weakest, about 59 percent of flat strength |
| Impact resistance | Good, flexes instead of snapping | Good, tougher than PLA on a notched test | Excellent, bends and returns to shape |
| Stiffness | Stiff with a little give | Rigid | Stiff, more flexible in thin layers |
| UV and weather resistance | Moderate | Excellent | Poor |
| Warping | Low to moderate | Moderate to high | High |
| Moisture sensitivity | Moderate | Low | Very high |
| Chemical resistance | Good | Good | Excellent |
| Wear resistance | Fair | Fair | Excellent, best for gears and hinges |
| Enclosure needed | No, optional | Recommended, near required | Required |
| Ventilation needed | No | Yes, styrene fumes | Good practice |
| Typical price per kilogram | Lowest of the three | Middle | Highest of the three |
Nylon wins flat by a wide margin and loses the most upright. PETG barely loses strength across the layers, so a PETG hook printed upright still holds while a nylon hook printed upright can snap. Turn the part so the main load runs along the layers. Heat figures agree on the order and disagree on the digits across brands, so use the order, not the digits.
Which filament wins for each drone and RC part?
Small frames, whoop frames, and prop guards. PETG first. It is the safest first plastic for a small frame, per the DroneTrader guide, and the default for whoop frames and prop guards, per the Prusa Knowledge Base summary in that guide. For larger builds, DroneTrader recommends a molded carbon kit for frame arms.
Mounts, brackets, and standoffs. PETG for rigid mounts indoors or in shade, ASA for mounts in sun. For a high-load bracket, nylon is the pick, but only after your own validation, per the ADP guide.
Outdoor parts, canopies, and housings. ASA, without a close second. Anything that lives outside, sits on a car dashboard, or flies in direct sun all summer belongs in ASA: antenna mounts, camera housings, field boxes, RC car bodies, and garden and automotive exterior parts. PETG ages faster in sun, PLA breaks down in sun, and nylon has poor UV resistance.
High-heat parts, motor mounts, and enclosures. ASA first, nylon second, and the stocked HT-PLA Pro as the easy option. Parts near motors and hot electronics need heat resistance PETG does not have. HT-PLA Pro prints like PLA with no enclosure and anneals at 100C for 30 minutes for its best heat resistance.
Gears, hinges, bushings, and wear parts. Nylon, and nothing else in this comparison. Its abrasion resistance and slipperiness are why gears, hinges, and living hinges are nylon jobs in every guide.
RC car and truck parts. PETG for brackets, chassis pieces, and guards that take hits. ASA for bodies and exterior parts in sun. Nylon for gears and suspension parts that wear.
What not to print. Print the parts that hold things. Buy the parts that spin or carry current. No filament here replaces a motor, a speed controller, a flight controller, a battery, or a propeller. Printed propellers are not a safe substitute for molded props. Bench-test every printed structural part with the propellers off, and check it for cracks after every hard landing.
What mistakes should you avoid?
- Jumping straight to nylon. Do not skip PETG and jump straight to nylon. The skills you build dialing in PETG transfer directly to the harder materials.
- Printing ASA without an enclosure or ventilation. ASA without an enclosure warps and splits, and without ventilation it fills the room with styrene fumes. Get the enclosure and the airflow first.
- Printing nylon wet. Wet nylon is the most common nylon failure. If you hear popping or see rough surfaces and weak layer bonds, the filament is wet. Dry it and print from a dry box. A strong material printed wet can end up weaker than dry PETG, per the 3DX guide.
- Buying on the flat tensile number alone. It is the most flattering value on the datasheet. For printed parts, the across-layer strength and the heat deflection figure usually decide whether a part survives, per the 3DX guide.
- Comparing brands’ datasheets directly. Test settings differ, so compare materials within one brand’s sheets, per the 3DX guide.
- Ignoring orientation. A part printed standing up, with the load pulling its layers apart, can snap where the same part printed lying down would hold. Think about the crash direction before you slice.
- Assuming carbon fiber means tougher. Fibers add stiffness, not toughness, and they wear brass nozzles, per the 3DX guide.
- Skipping the test fit. Print a fit check in PLA or PLA+ before committing to a long ASA or nylon print. A fit check that fails costs minutes instead of hours.
Why is my print failing?
| Problem | Likely cause | Fix |
|---|---|---|
| Warping, corners lifting | Cold bed, drafts, no enclosure | Raise the bed temperature, add a 5 to 10 mm brim, close the enclosure. |
| Layer splitting or cracking | Too much cooling, low nozzle temperature, cold chamber | Reduce the fan to near zero for ASA and nylon, raise the nozzle temperature 5 to 10C, keep the enclosure warm. |
| Stringing | Wet filament, high temperature | Dry the spool, lower the temperature, tune retraction. |
| Popping, bubbles, rough surfaces | Moisture in the filament | Dry the spool fully. For nylon, dry 70 to 80C for 6 to 12 hours and print from a dry box. |
| Poor bed adhesion | Dirty bed, wrong bed temperature, wrong surface | Clean the bed with isopropyl alcohol, re-level, use glue stick on smooth PEI. Nylon usually needs Garolite or PVA glue. |
| Part snaps along a layer line | Load across the layers, weak layer bonding | Reorient the part so the load runs along the layers, reduce the fan, add walls. |
| ASA part smells and the room feels stuffy | Styrene fumes, no ventilation | Stop the print, ventilate the room, and do not print ASA again without a carbon filter. |
| Nylon part warps on a large flat print | No enclosure, damp filament, wrong bed surface | Enclose the printer, dry the filament, use a large brim and a Garolite bed surface. |
Which filament should you buy?
First functional part, open-frame printer, most RC and drone parts. Buy PETG. It prints without an enclosure, flexes instead of snapping, and covers guards, brackets, chassis pieces, and mounts. The stocked PETG refill is the Anycubic PETG Filament Refill, 1.75mm, 1KG (ID 17689) at $18.99. It is a refill coil only with no spool included, so you need a reusable spool.
Part that lives outdoors, sits in sun, or sits in a hot car. Buy ASA. No ASA filament is stocked at the time of writing, so there is no ASA product link in this guide. Buy ASA from a filament maker whose datasheet you have read, and print it enclosed and ventilated.
High-load bracket, gear, hinge, or wear part, and you own an enclosure and a dryer. Buy nylon. No nylon filament is stocked at the time of writing, so there is no nylon product link in this guide. Buy the grade that matches the job, PA6 for strength, PA12 for lower moisture absorption, and dry it before every print.
Hot spot near a motor or electronics, and you want the easy option. Buy HT-PLA Pro. The stocked Polymaker HT-PLA Pro Filament, 1.75mm, 1KG (ID 17644) is $29.99. It prints like PLA with no enclosed chamber and anneals at 100C for 30 minutes for its best heat resistance.
FAQ
Which filament is strongest, PETG, ASA, or nylon? Nylon is the strongest common FDM filament overall, especially in carbon fiber filled form. On an open-frame printer, PETG is the strongest practical pick, because it needs no enclosure. Source: Techietory FAQ section, 3DX FAQ section.
Is ASA better than PETG for outdoor parts? Yes. ASA resists UV light and weathering far better than PETG, so it keeps its color and structure outdoors while PETG ages faster in sun. PETG is easier to print and stronger across the layers, so use PETG indoors and ASA outside. Source: Techietory FAQ section, Filwiz material comparison.
Do I need an enclosure to print ASA or nylon? Yes, for reliable results. An enclosure holds a stable chamber temperature of roughly 40 to 60C, which reduces warping and layer splitting. ASA warps significantly without one, and nylon warps severely without one. PETG prints fine without one. Source: Techietory FAQ section, Filwiz enclosure guide.
Can I print nylon without drying it first? No. Nylon absorbs moisture from the air within hours, and wet nylon prints with bubbles, rough surfaces, and weak layer bonds. Dry it at 70 to 80C for 8 to 12 hours before printing, store it sealed with desiccant, and print from a dry box when possible. Source: Techietory nylon section, Filwiz nylon section.
Which filament should I use for a drone frame? PETG for a small frame, such as a whoop. ASA for a frame or canopy that lives outdoors in sun. Nylon or carbon fiber nylon only for high-load prototypes, and only after your own validation. For frame arms on a large build, a molded carbon kit is the safer buy. Source: ADP quick reference, DroneTrader component matrix.
Is PETG stronger than PLA? PETG is tougher, more heat resistant, and more chemically resistant than PLA, and it flexes instead of shattering. PLA is stiffer and better for visual models. In Bambu Lab datasheet figures, PETG Basic beats PLA Basic on tensile strength, impact strength, and heat resistance, but other brands publish different numbers. Source: Techietory FAQ section, 3DX FAQ section.
Can you print an entire drone? No. You can print the frame, mounts, prop guards, and battery holders, but motors, flight controllers, speed controllers, batteries, and propellers must be bought. Printed parts hold things; they do not spin or carry current. Source: DroneTrader FAQ section.
Parts used in this guide
Prices and stock were verified live on qualityrcparts.com on 2026-11-21. Both items below are in stock and purchasable. No ASA filament and no nylon filament is stocked at the time of writing: a store search for “asa” returns 0 products, a store search for “nylon filament” returns 0 products, and a store search for “filament” returns 9 products, none of them ASA or nylon filament. The nylon search results are hardware, such as nylon screws, standoffs, propellers, and hinges, not filament. No ASA or nylon product is linked because none exists.
- Anycubic PETG Filament Refill, 1.75mm, 1KG (ID 17689) – $18.99. Refill coil only, no spool included. Impact resistance twice that of standard PLA per the listing, 1.75mm diameter, 1KG. The PETG pick in this guide.
- Polymaker HT-PLA Pro Filament, 1.75mm, 1KG (ID 17644) – $29.99. Full 1KG spool. Prints like PLA with no enclosed chamber and no hardened nozzle needed, anneals at 100C for 30 minutes for its best heat resistance. The stocked heat-resistant option for hot spots in this guide.
Shipped fast and securely from our secure facility in Queensbury, NY. QRC ships within the USA only.
Related guides
- PLA vs PLA+ vs PETG: Pick the Right 3D Printer Filament for Drone Parts
- Best FPV Drone Frames in the USA
- Best Filament FPV Drone Builders Use for Frames and Mounts
- How to Store Filament So It Stays Dry and Prints Clean
- Filament Refill vs Spool: How Anycubic Refills Save You Money
- FPV Drone Repair Parts: Print Your Own Replacements
- HT-PLA Pro: A Heat Resistant Filament for Enclosures and Hot Builds
Sources
- Quality RC Parts, PLA vs PLA+ vs PETG: Pick the Right 3D Printer Filament for Drone Parts: https://qualityrcparts.com/pla-vs-pla-plus-vs-petg-drone-parts/
- Quality RC Parts, Best FPV Drone Frames in the USA: https://qualityrcparts.com/best-fpv-drone-frames-usa/
- Quality RC Parts, Best Filament FPV Drone Builders Use for Frames and Mounts: https://qualityrcparts.com/best-filament-fpv-drone-frames-mounts/
- Quality RC Parts, How to Store Filament So It Stays Dry and Prints Clean: https://qualityrcparts.com/how-to-store-filament-stays-dry/
- Quality RC Parts, Filament Refill vs Spool: How Anycubic Refills Save You Money: https://qualityrcparts.com/filament-refill-vs-spool-save-money/
- Quality RC Parts, HT-PLA Pro: A Heat Resistant Filament for Enclosures and Hot Builds: https://qualityrcparts.com/ht-pla-pro-heat-resistant-filament/
- Quality RC Parts store listings, checked live 2026-11-21 (IDs 17689, 17644; store searches for “asa”, “nylon filament”, “filament”)
- Filwiz, Engineering Filaments: PETG, ASA, and Nylon: https://filwiz.com/guides/petg-asa-nylon-engineering-filaments-guide
- ADP Industries, Best Filament for 3D Printed Drone Parts: The Complete Material Guide for FPV Pilots: https://adpindustries.com/blog/best-filament-3d-printed-drone-parts/
- Techietory, The Complete Filament Guide: PLA, PETG, ABS, ASA, TPU, and Nylon Compared: https://techietory.com/3d-printer-filament-guide-pla-petg-abs-asa-tpu-nylon/
- CadFlow, 3D printer filament types compared: PLA, PETG, ABS, ASA, TPU and nylon: https://www.cadflow.app/blog/3d-printer-filament-types/
- 3DX, High-strength filament: compare PETG, ASA, PC and CF nylon: https://3dx.info/high-strength-3d-printing-filament/
- DroneTrader, 3D Printed Drone: What to Print, Which Filament and Where It Fails: https://blog.dronetrader.com/3d-printed-drone/
- Polymaker technical data sheets, as compared by CadFlow (PolyLite PLA, PETG, PolyLite ABS, ASA, PolyFlex TPU95, PolyMide CoPA)
- Bambu Lab technical data sheets, as compared by 3DX (PLA Basic, PETG Basic, ABS, ASA, PC, PAHT-CF)
- Prusa Knowledge Base material pages (PLA, PETG, ASA, polyamide nylon), as summarized by DroneTrader
Last updated: 2026-11-21